3D Lab secures US patent for ultrasonic metal atomisation technology

September 19, 2024

3D Lab has been granted a USA Patent for its “Method and Device for Producing Heavy Metal Powders by Ultrasonic Atomization” innovation (Courtesy 3D Lab)
3D Lab has been granted a USA Patent for its “Method and Device for Producing Heavy Metal Powders by Ultrasonic Atomization” innovation (Courtesy 3D Lab)

3D Lab sp zoo, based in Warsaw, Poland, has been granted a US patent for its “Method and Device for Producing Heavy Metal Powders by Ultrasonic Atomization” innovation. This new patent further strengthens 3D Lab’s growing intellectual property portfolio and highlights its ultrasonic metal atomisation capabilities.

This US patent is the latest success in a series of submitted patent applications, following the recent Chinese Patent granted for metal powder production technology.

THE WORLD OF POWDER METALLURGY TO YOUR INBOX
Subscribe to our weekly newsletter
Sign up

The patented technology is at the core of the company’s ATO series of ultrasonic metal atomisers. This technology produces high-quality spherical metal powders with precise control over particle size, excellent flowability, and low oxygen content. These characteristics are critical for Additive Manufacturing and various industrial applications.

“We are proud to add this USA patent to our rapidly growing portfolio of global intellectual property. Our patented technologies drive our mission to provide advanced and versatile solutions for metal powder production, ensuring superior material quality and accelerating material innovations. This patent is a significant milestone in our journey, reflecting the dedication and innovative spirit of our team,” shared Jakub Rozpendowski CEO of 3D Lab.

ATO Lab Plus Ultrasonic metal atomiser

The ATO Lab Plus is an advanced ultrasonic metal atomiser designed for lab-scale production of metal powders. Ideal for research and production environments, it enables the efficient and cost-effective production of reactive and non-reactive metal powders.

The atomiser has a modular construction, allowing for easy expansion of powder production capabilities through the use of the interchangeable modules. The device has advanced safety systems and automatic features, offering a versatile solution for producing metal powder.

metalatomizer.com/en

Download PM Review magazine

In the latest issue of PM Review…

Download PDF

Extensive Powder Metallurgy industry news coverage, and the following exclusive deep-dive articles and reports:

  • Powder Metallurgy: Discover innovative technologies meeting the demands of vehicle electrification
  • Gevorkyan a.s.: Europe’s fast-growing Powder Metallurgy company achieving success through a diversified customer base
  • Powder Metallurgy in Asia: A status update from the World PM2024 Congress, Yokohama

The latest news from the world of metal powders, delivered to your inbox

Don't miss any new issue of PM Review, and get the latest industry news. Sign up to our weekly newsletter.

Sign up

Join our community

Discover our magazine archive…

The free-to-access PM Review magazine archive offers unparalleled insight into the world of Powder Metallurgy from a commercial and technological perspective through:

  • Reports on visits to leading PM part manufacturers, metal powder manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

 

Browse the archive

 

Looking for PM production equipment, metal powders, R&D support and more?

Discover suppliers of these and more in our
advertisers’ index and buyer’s guide, available in the back of PM Review magazine.

  • Powders & materials
  • Powder process, classification & analysis
  • PM products
  • Atomisers & powder production technology
  • Compaction presses, tooling & ancillaries
  • Sintering equipment & ancillaries
  • Post-processing
  • Consulting & toll sintering
View online
Share via
Copy link